A one-page review of tablet manufacturing for Pharm.D students: the steps from powder to tablet, what each excipient does, pharmacopoeial QC tests, and common tablet and coating defects with their fixes.
- Diluents (fillers): Lactose, MCC, mannitol, dicalcium phosphate: add bulk
- Binders: PVP, starch paste, HPMC: hold granules together
- Disintegrants: Starch; superdisintegrants croscarmellose, sodium starch glycolate, crospovidone: break tablet apart
- Lubricants: Magnesium stearate, stearic acid: stop sticking to punches (over-mixing slows dissolution)
- Glidants: Colloidal silicon dioxide, talc: improve powder flow
- Coatings: Film (HPMC), enteric (cellulose acetate phthalate, methacrylate copolymers), sugar coating
- Wet granulation: Best for poorly flowing or low-density powders; not for moisture/heat-sensitive drugs
- Dry granulation: Roller compaction or slugging; for moisture-sensitive drugs
- Direct compression: Fewest steps and cheapest; needs good flow and compressibility
- Weight variation: Individual tablet weights within pharmacopoeial limits
- Content uniformity: Each tablet has the right amount of drug (low-dose tablets)
- Hardness: Breaking force, typically 4–10 kg (40–100 N)
- Friability: Weight loss after tumbling ≤ 1%
- Disintegration (BP): Uncoated ≤ 15 min, film-coated ≤ 30 min; enteric: intact in acid for 2 h, then disintegrate in buffer within 60 min
- Dissolution: % drug released over time: the key test linked to bioavailability
- Capping: Top separates as a cap: air trapped, too many fines, too dry granules, high speed → add binder, pre-compression, slow press
- Lamination: Splits into layers: similar causes to capping, worn tooling
- Sticking / picking: Material sticks to punch faces or lettering: wet granules, low lubricant → dry granules, more lubricant, polish punches
- Chipping & cracking: Damaged edges or cracks: worn punches, too hard or too dry
- Mottling: Uneven colour: dye migration, poor mixing
- Binding: Tablet sticks in die: insufficient lubricant
- Orange peel: Rough surface: spray too viscous or drying too fast
- Blistering: Bubbles under coat: drying too hot
- Twinning: Tablets stuck together: too much spray, slow pan speed
- Logo bridging: Coat fills the logo: poor film adhesion, high plasticiser
- Cracking: Coat splits: too little plasticiser
- Principles: Right people, premises, processes, documentation and validation
- Regulators: WHO GMP, DRAP (Pakistan), FDA cGMP, EU GMP
- Key documents: Batch manufacturing record, SOPs, certificate of analysis
- Deviations: Investigate, document, CAPA (corrective and preventive action)
From powder to packed tablet
Flow chart drawn for this blog.
Practical points for students
Pakistan has a large pharmaceutical manufacturing sector, and many Pharm.D graduates start their careers in production or quality control. Interviews often ask about granulation methods, excipient roles and the causes of capping and sticking, so this card doubles as interview preparation.
Important: this card is for education and revision. Treatment decisions must follow local guidelines and the treating doctor. More pocket cards: Pharmaceutics Review | Clinical Pocket Cards | Disease Pocket Cards